~(169)Er-FHMA的制备

The Preparation of ~(169)Er-FHMA

  • 摘要: 利用天然丰度Er2O3(光谱纯)作靶料,经反应堆辐照后,用HNO3溶解生成169Er(NO3)3。在0.9%NaCl介质中,加入FeSO4、NaOH和稳定剂PVP(聚乙烯吡咯烷酮)经超声波分散,获得69Er-FHMA(氢氧化铁聚合体),用莱之超显微镜观察测定其粒径为3~8μm,实验表明169Er-FHMA在0.9%NaCl溶液中溶出率基本不受温度影响。

     

    Abstract: The natural abundance Er2O3 is taken as the target,irradiated by reactor,and generated 169Er(NO3)3 solved in HNO3. In the medium of 0.9% NaCl,FeSO4,NaOH and the stable reagent of PVP is added while be keeping the definite acidity. The 169ErFHMA(Fe(OH)3 polymer) is gained after the dispersal by supersonic. The size of particles is 3~8 μm, the temprature is no effect on dissolve rate of 19ErFHMA in 0.9% NaCl solution.

     

/